首页 > SPI 模具表面抛光标准

SPI 模具表面抛光标准

2020-09-17 1页 xls 18KB 59阅读

用户头像 个人认证

橙子到此一游

暂无简介

举报
SPI 模具表面抛光标准Blad1 OverviewSPIstandardforpolishing Philips SPI SPI Discription Rainµm Comments standard (old) (new) (DIN) 0-UN-D249 1 A-1 Diamondbuffgrade3 0-0.025 Formirrororopticalfinishes.Mosttimeconsuming.Steelgradeimportanttoresults 1-UN-D249 A-2 Diamondbuffgrade6...
SPI 模具表面抛光标准
Blad1 OverviewSPIstandardforpolishing Philips SPI SPI Discription Rainµm Comments standard (old) (new) (DIN) 0-UN-D249 1 A-1 Diamondbuffgrade3 0-0.025 Formirrororopticalfinishes.Mosttimeconsuming.Steelgradeimportanttoresults 1-UN-D249 A-2 Diamondbuffgrade6 0.025-0.05 2 A-3 Diamondbuffgrade15 0.05-0.076 B-1 600gritpaper 0.05-0.076 Removesalltoolandmachiningmarks.Providesgoodmouldrelease.Lightreflectingfinishonmouldedpart,somesheen. 2-UN-D249 B-2 400gritpaper 0.10-0.127 3-UN-D249 3 B-3 320gritpaper 0.23-0.25 C-1 600stone 0.25-0.30 Removesalltoolandmachiningmarks.Providesgoodmouldrelease.Mutefinishonmouldedpart,nosheen. C-2 400stone 0.64-0.71 C-3 320stone 0.97-1.07 4-UN-D249 0.40 TechnicalSmooth,polishingonlyneededforpropermouldingfunction 4 Nomoreinuse. D-1 Dryblastglassbead11,200distanceat0.7Mpa;5sec 0.25-0.30 Fordecorativefinishes.Oftenusedfordiecastandthermosetcooling.Helpshideshrinkmarksandotherimperfections.Dull,nonreflectingfinishonmouldedorcastpart. 5 D-2 Dryblast240oxyde,125distanceat0.7Mpa;5sec 0.66-0.81 D-3 Dryblast240oxyde,150distanceat0.7Mpa;5sec 4.83-5.84Blad2 Blad3
/
本文档为【SPI 模具表面抛光标准】,请使用软件OFFICE或WPS软件打开。作品中的文字与图均可以修改和编辑, 图片更改请在作品中右键图片并更换,文字修改请直接点击文字进行修改,也可以新增和删除文档中的内容。
[版权声明] 本站所有资料为用户分享产生,若发现您的权利被侵害,请联系客服邮件isharekefu@iask.cn,我们尽快处理。 本作品所展示的图片、画像、字体、音乐的版权可能需版权方额外授权,请谨慎使用。 网站提供的党政主题相关内容(国旗、国徽、党徽..)目的在于配合国家政策宣传,仅限个人学习分享使用,禁止用于任何广告和商用目的。

历史搜索

    清空历史搜索